(All numbering and residues are taken from first PDB file)
Bending Residue Dihedral Analysis
Residue
iResidue
i+1Distance of hinge axis to residue i in
(A) Distance of hinge axis to residue i in
(A) Change in
(deg) Change in
(deg) Angle of psi(i) axis to hinge axis
(deg) Angle of psi(i) axis to hinge axis
(deg) Percentage Progress
LYS-140
PRO-141
3.1
3.1
-0.5
-1.0
124.0
122.0
-13.2
PRO-141
PHE-142
1.5
1.4
-2.6
4.7
122.2
122.5
53.2
PHE-142
TYR-143
4.7
4.6
-0.2
-1.8
126.3
127.1
-132.4
TYR-143
GLU-144
4.7
4.6
2.7
0.9
110.8
109.0
40.4
GLU-144
ASP-145
5.2
5.1
-0.8
-2.6
51.2
53.5
43.5
Graph shows rotational transition at bending residues and can be used
to identify hinge bending residues.
Probably only informative for interdomain rotations greater than 20 degrees
Residue
iResidue
i+1Distance of hinge axis to residue i in
(A) Distance of hinge axis to residue i in
(A) Change in
(deg) Change in
(deg) Angle of psi(i) axis to hinge axis
(deg) Angle of psi(i) axis to hinge axis
(deg) Percentage Progress
SER-158
LEU-159
18.2
18.2
3.2
-1.0
98.1
102.5
37.2
LEU-159
LEU-160
18.1
18.2
-6.6
10.6
141.6
138.5
47.5
LEU-160
ALA-161
16.1
16.2
2.0
-1.2
29.8
31.0
-0.5
ALA-161
CYS-162
17.6
17.9
-4.6
-1.2
90.2
85.2
58.2
CYS-162
ASP-163
21.2
21.4
26.3
-24.7
33.2
42.8
-42.1
ASP-163
GLN-164
22.0
22.0
-6.9
-3.8
148.2
151.1
-287.8
ASP-163
GLN-164
22.0
22.0
-6.9
-3.8
148.2
151.1
-287.8
Graph shows rotational transition at bending residues and can be used
to identify hinge bending residues.
Probably only informative for interdomain rotations greater than 20 degrees
Residue
iResidue
i+1Distance of hinge axis to residue i in
(A) Distance of hinge axis to residue i in
(A) Change in
(deg) Change in
(deg) Angle of psi(i) axis to hinge axis
(deg) Angle of psi(i) axis to hinge axis
(deg) Percentage Progress
ASP-163
GLN-164
22.0
22.0
-6.9
-3.8
148.2
151.1
-287.8
ASP-163
GLN-164
22.0
22.0
-6.9
-3.8
148.2
151.1
-287.8
GLN-164
ASP-165
19.9
19.9
3.7
14.4
19.8
23.4
620.7
ASP-165
VAL-166
22.2
22.3
-17.4
8.4
113.7
124.8
-278.3
VAL-166
ALA-167
22.8
22.8
2.0
1.6
106.6
101.6
-176.2
ALA-167
PHE-168
20.5
20.6
7.3
-3.6
51.7
52.7
-28.5
PHE-168
ASP-169
17.8
17.9
12.1
-2.9
19.1
20.6
305.4
Graph shows rotational transition at bending residues and can be used
to identify hinge bending residues.
Probably only informative for interdomain rotations greater than 20 degrees
Residue
iResidue
i+1Distance of hinge axis to residue i in
(A) Distance of hinge axis to residue i in
(A) Change in
(deg) Change in
(deg) Angle of psi(i) axis to hinge axis
(deg) Angle of psi(i) axis to hinge axis
(deg) Percentage Progress
ILE-250
LEU-251
7.0
6.8
-0.1
0.6
163.0
164.1
25.5
LEU-251
SER-252
7.5
7.4
-3.0
3.2
109.8
110.0
-24.8
SER-252
PHE-253
10.4
10.3
0.8
1.5
6.1
6.5
55.5
Graph shows rotational transition at bending residues and can be used
to identify hinge bending residues.
Probably only informative for interdomain rotations greater than 20 degrees
Residue
iResidue
i+1Distance of hinge axis to residue i in
(A) Distance of hinge axis to residue i in
(A) Change in
(deg) Change in
(deg) Angle of psi(i) axis to hinge axis
(deg) Angle of psi(i) axis to hinge axis
(deg) Percentage Progress
LEU-255
LEU-256
8.7
9.0
-1.4
-2.0
32.2
31.1
104.4
LEU-256
ASN-257
11.1
11.2
0.6
-1.3
142.9
142.5
2.3
ASN-257
TRP-258
8.0
8.1
1.0
-0.4
108.8
109.0
1.8
Graph shows rotational transition at bending residues and can be used
to identify hinge bending residues.
Probably only informative for interdomain rotations greater than 20 degrees
Residue
iResidue
i+1Distance of hinge axis to residue i in
(A) Distance of hinge axis to residue i in
(A) Change in
(deg) Change in
(deg) Angle of psi(i) axis to hinge axis
(deg) Angle of psi(i) axis to hinge axis
(deg) Percentage Progress
ILE-282
HIS-283
11.7
11.6
-0.7
-2.2
97.3
97.6
-28.2
HIS-283
GLU-284
13.7
13.6
6.2
-5.3
12.1
10.7
95.3
GLU-284
ARG-285
15.4
15.3
1.5
-6.9
87.7
88.0
31.1
Graph shows rotational transition at bending residues and can be used
to identify hinge bending residues.
Probably only informative for interdomain rotations greater than 20 degrees
Residue
iResidue
i+1Distance of hinge axis to residue i in
(A) Distance of hinge axis to residue i in
(A) Change in
(deg) Change in
(deg) Angle of psi(i) axis to hinge axis
(deg) Angle of psi(i) axis to hinge axis
(deg) Percentage Progress
ALA-311
LEU-312
14.0
14.1
-0.7
6.5
150.4
152.6
162.0
LEU-312
ARG-313
16.3
16.3
0.6
-1.2
72.0
75.2
58.0
ARG-313
THR-314
17.8
17.8
-7.8
0.1
120.6
120.4
-284.8
THR-314
ARG-315
21.3
21.5
3.7
-11.6
22.4
29.4
181.0
Graph shows rotational transition at bending residues and can be used
to identify hinge bending residues.
Probably only informative for interdomain rotations greater than 20 degrees
Residue
iResidue
i+1Distance of hinge axis to residue i in
(A) Distance of hinge axis to residue i in
(A) Change in
(deg) Change in
(deg) Angle of psi(i) axis to hinge axis
(deg) Angle of psi(i) axis to hinge axis
(deg) Percentage Progress
ARG-333
GLN-334
20.7
20.8
-8.4
5.7
143.8
144.3
-67.4
GLN-334
LEU-335
22.9
22.8
-3.2
-1.5
77.6
74.8
156.9
LEU-335
PRO-336
22.5
22.3
2.1
-1.3
68.2
68.6
-36.3
PRO-336
SER-337
25.5
25.2
9.8
-0.2
41.6
48.5
422.6
SER-337
PRO-338
25.8
25.5
1.5
-0.4
85.7
91.7
51.7
PRO-338
THR-339
28.9
28.0
12.8
-20.7
40.0
44.7
-326.2
THR-339
ILE-340
28.6
27.7
-2.3
6.5
131.2
132.7
26.9
ILE-340
PRO-341
28.9
28.2
-4.9
-0.7
76.2
76.7
38.9
PRO-341
TYR-342
28.7
28.3
-2.6
4.3
118.6
124.3
-20.2
TYR-342
ASP-343
25.0
24.8
9.1
-7.4
138.4
134.7
-0.9
ASP-343
LEU-344
24.2
24.0
3.3
-7.4
93.2
94.6
-103.8
Graph shows rotational transition at bending residues and can be used
to identify hinge bending residues.
Probably only informative for interdomain rotations greater than 20 degrees
Residue
iResidue
i+1Distance of hinge axis to residue i in
(A) Distance of hinge axis to residue i in
(A) Change in
(deg) Change in
(deg) Angle of psi(i) axis to hinge axis
(deg) Angle of psi(i) axis to hinge axis
(deg) Percentage Progress
SER-345
LEU-346
19.3
19.3
0.3
-7.8
70.6
70.7
-17.5
LEU-346
LEU-347
16.5
16.4
-1.3
3.3
105.7
108.4
0.6
LEU-347
VAL-348
15.7
15.6
4.3
-3.5
51.1
51.1
4.8
Graph shows rotational transition at bending residues and can be used
to identify hinge bending residues.
Probably only informative for interdomain rotations greater than 20 degrees